(888) 722-8260 | sales@diversifiedbronze.com | Cart
Custom Machining View Capabilities →

C67300

Leaded Manganese Bronze

Manganese Bronzes Wrought

Free-machining wrought manganese bronze. Combines high strength with the best machinability in the manganese bronze family.

Tensile Strength
55–80 ksi
Yield Strength
25–60 ksi
Machinability
70 / 100
Density
0.302 lb/in³

Chemical Composition

Element Min % Max %
Copper (Cu) 58 63
Zinc (Zn) Remainder
Manganese (Mn) 2 3.5
Silicon (Si) 0.5 1.5
Lead (Pb) 0.4 3
Iron (Fe) 0.5

Physical Properties

Density 0.302 lb/cu in
Specific Gravity 8.36
Melting Point (Solidus) 1590°F
Melting Point (Liquidus) 1625°F
Electrical Conductivity 20% IACS

Mechanical Properties

Tensile Strength 55–80 ksi
Yield Strength 25–60 ksi
Elongation 15–30%
Hardness 60–90 Rockwell B
Machinability Rating 70

Thermal Properties

Thermal Conductivity 51 Btu/ft·hr·°F
Coefficient of Expansion 11.8 × 10⁻⁶ /°F
Specific Heat 0.09 Btu/lb·°F

Fabrication Properties

Soldering Good
Brazing Good
Oxyacetylene Welding Fair
Gas Shielded Arc Fair
Coated Metal Arc Fair
Cold Working Fair
Hot Forming Excellent

Typical Applications

  • Bushings and bearing sleeves
  • Gear components
  • Valve stems
  • Hydraulic cylinder parts
  • Wear strips
  • Shafting

Applicable Specifications

  • SAE J461
  • SAE J463