Heat-treatable copper-nickel-silicon alloy. Age hardening roughly doubles its strength while keeping useful electrical conductivity.

Tensile Strength
50–100 ksi
Yield Strength
20–80 ksi
Machinability
30 / 100
Density
0.318 lb/in³

Chemical Composition

Element Min % Max %
Copper (Cu) Remainder
Nickel (Ni) 1.6 2.2
Silicon (Si) 0.4 0.8
Zinc (Zn) 0.5
Iron (Fe) 0.1

Physical Properties

Density 0.318 lb/cu in
Specific Gravity 8.81
Melting Point (Solidus) 1940°F
Melting Point (Liquidus) 1985°F
Electrical Conductivity 40% IACS

Mechanical Properties

Tensile Strength 50–100 ksi
Yield Strength 20–80 ksi
Elongation 6–32%
Hardness 25–95 Rockwell B
Machinability Rating 30

Thermal Properties

Thermal Conductivity 75 Btu/ft·hr·°F
Coefficient of Expansion 9.9 × 10⁻⁶ /°F
Specific Heat 0.09 Btu/lb·°F

Fabrication Properties

Soldering Excellent
Brazing Excellent
Oxyacetylene Welding Fair
Gas Shielded Arc Good
Coated Metal Arc Fair
Cold Working Excellent
Hot Forming Good

Typical Applications

  • High-strength fasteners
  • Electrical connectors
  • Spring components
  • Valve stems
  • Small-diameter bushings
  • Aerospace hardware

Applicable Specifications

  • ASTM B411
  • SAE J461
  • SAE J463