C64200

Silicon Aluminum Bronze

Aluminum Bronzes Wrought

Best machinability of aluminum bronzes. The silicon addition improves machining while maintaining corrosion resistance.

Tensile Strength
70–85 ksi
Yield Strength
28–50 ksi
Machinability
60 / 100
Density
0.278 lb/in³

Chemical Composition

Element Min % Max %
Copper (Cu) 89.5 92
Aluminum (Al) 6.3 7.6
Silicon (Si) 1.5 2.2
Iron (Fe) 0.3
Tin (Sn) 0.2

Physical Properties

Density 0.278 lb/cu in
Specific Gravity 7.69
Melting Point (Solidus) 1840°F
Melting Point (Liquidus) 1880°F
Electrical Conductivity 7% IACS

Mechanical Properties

Tensile Strength 70–85 ksi
Yield Strength 28–50 ksi
Elongation 20–35%
Hardness 65–85 Rockwell B
Machinability Rating 60

Thermal Properties

Thermal Conductivity 21 Btu/ft·hr·°F
Coefficient of Expansion 9.5 × 10⁻⁶ /°F
Specific Heat 0.09 Btu/lb·°F

Fabrication Properties

Soldering Good
Brazing Good
Oxyacetylene Welding Good
Gas Shielded Arc Excellent
Coated Metal Arc Good
Cold Working Fair
Hot Forming Good

Typical Applications

  • Valve stems
  • Fasteners
  • Hardware
  • Bushings
  • Screw machine products
  • Marine components

Applicable Specifications

  • ASTM B150
  • SAE J461
  • SAE J463